Citation link: http://dx.doi.org/10.25819/ubsi/10400
Files in This Item:
File Description SizeFormat
Stennei_Einfluss_der_Herstellungsroute.pdf693.79 kBAdobe PDFThumbnail
View/Open
Dokument Type: InProceedings
metadata.dc.title: Einfluss der Herstellungsroute auf die Umformbarkeit von Cr-Mn-Verbundwerkstoffen für das Presshärten
Authors: Stennei, Markus 
Grodotzki, Joshua 
Tekkaya, A. Erman 
Institute: Institut für Produktionstechnik 
Free keywords: Presshärten, Wärmebehandlung, Verbundwerkstoffe, Biegeversuche
Dewey Decimal Classification: 620 Ingenieurwissenschaften und zugeordnete Tätigkeiten
GHBS-Clases: ZIR
Issue Date: 2023
Publish Date: 2023
Source: Engel, Bernd (Hrsg.): Transformation in der Biegetechnik : Tagungsband zum 6. Biegeforum Siegen : 24.-31. März 2023. Siegen: universi - Universitätsverlag Siegen, 2023. - ISBN 978-3-96182-155-6 - DOI http://dx.doi.org/10.25819/ubsi/10365, S. 115-122
Abstract: 
The analysis of bending properties of a new composite material for press hardening is presented in this paper. This composite material consists of a boron-Magan core (22MnB5) and a stainless-steel cover layer. The core material is the typical press hardening material for industrial applications. Two different types of top layer are considered, an austenitic (1.4301) and a martensitic (1.4021) stainless steel.
Initial investigations have shown that the manufacturing of the roll clad semi-finished product leads to low the formability of the cover layer materials. In this analysis, different heat treatment strategies have been added to the process route and their influence on the formability is investigated. For this purpose, a 3-point bending test with optical strain measurement system is developed. The test setup allows the accurate determination of the strain at failure of the cover layer at room temperature. It is shown that neither heat treatment after hot rolling nor intermediate annealing during cold rolling improves formability. The highest degree of forming on the outer bend is obtained with a process route without heat treatment. Even in this particular case, the remaining formability is about 50 % lower compared with the values achieved by the untreated material of the cover layer. No reduction in bond strength due to heat treatment was observed. The formability results indicate that further analysis of the entire process chain and the associated diffusion processes is necessary to understand the remaining underperformance of the composite material.
DOI: http://dx.doi.org/10.25819/ubsi/10400
URN: urn:nbn:de:hbz:467-26120
URI: https://dspace.ub.uni-siegen.de/handle/ubsi/2612
License: http://creativecommons.org/licenses/by-sa/4.0/
Appears in Collections:Universi

This item is protected by original copyright

Show full item record

Page view(s)

266
checked on Dec 26, 2024

Download(s)

82
checked on Dec 26, 2024

Google ScholarTM

Check

Altmetric


This item is licensed under a Creative Commons License Creative Commons